BC-55/65 Degradable material zipper bag blowing machine
Main Parameters:
Model | BC-55 | BC-65 | BC-85 |
Raw Material | LDPE(density0.921) | LDPE(density0.921) | LDPE(density0.921) |
Width | 50-450mm | 50-550mm | 50-750mm |
Thickness | 0.03-0.10mm | 0.03-0.10mm | 0.03-0.10mm |
Screw | Φ45 | Φ55 | Φ65 |
LD | 30:1 | 30;1 | 30:1 |
Main power | 7.5kw | 7.5kw | 15kw |
Vice power | 1.5kw | 1.5kw | 2.2kw |
Heart | 12kw | 15kw | 18kw |
Cooling | 1.1kw | 1.5kw | 2.2kw |
Total power | 25kw | 28kw | 30kw |
Voltage | 50Hz-60Hz 380V | 50Hz-60Hz 380V | 50Hz-60Hz 380V |
Output | 5-35kg/h | 5-35kg/h | 5-45kg/h |
Dimension (L×W×H) | 6000×1600×4500mm | 6000×1600×4500mm | 6000×1600×4500mm |
Weight | 1500kg | 1800kg | 2000kg |
Common faults and solutions of self sealing bag blowing machine
Difficulty in drawing mold for self sealing bag blowing machine:
(1) Improper temperature control of the machine head: The machine head temperature should be adjusted appropriately.
(2) Uneven discharge of the mold: The gap between the molds should be adjusted while adjusting the temperature of the machine head connector appropriately.
(3) The molten material contains impurities of coke: purify the raw materials and clean the machine head and screw.
(4) Improper control of extrusion process conditions: The process conditions should be adjusted appropriately.
Self sealing bag blown film machine bubble tube skewed:
(1) The temperature of the body and mold is too high: reduce it appropriately.
(2) The temperature of the machine head connector is too high: reduce it appropriately.
(3) Uneven discharge of the mouth mold and uneven thickness of the film: adjust the gap between the mouth mold and the temperature of the machine head connector appropriately.